Rubber compound for hoses of turbine boosters

No.

Test item

Performance indexes        (inner layer)

Performance indexes      (external layer)

1

Hardness (Shores A)                  Degree

55±5 or drawing

55±5 or drawing

2

Tensile strength                     MPa

≥10.0

≥10.0

3

Elongation at break                   %

200~600

200~600

4

Tear strength DIN ISO34-1 method A          kN/m

≥5.0

≥5.0

5

Heat resistance 125℃×94h    

Tensile strength    Degree

0~+6

0~+6

Elongation at break    MPa

≥9.0

≥9.0

Tear strength           %

180~550

180~550

Tear strength         kN/m

≥4.0

≥4.0

6

Heat resistance 110℃×504h    

Change in hardness Degree

0~+8

0~+8

Tensile strength     MPa

≥9.0

≥9.0

Elongation atbreak     %

180~550

180~550

7

Oil resistance 125℃×94h     

Change in hardness Degree

-8~+8

/

Elongation at break   MPa

≥9.0

/

Tear strength            %

≥150

/

Mass change ratio       %

-4~+8

/

Tear strength         N/m

≥2.5

/

8

Oil resistance 110℃×504h    

Change in hardness Degree

-8~+10

/

Tensile strength      MPa

≥9.0

/

Elongation at break     %

≥140

/

Mass change ratio       %

-4~+10

/

9

Diesel resistance23℃×46h     

Change in hardness Degree

/

-20~0

Tensile strength      MPa

/

6

Elongation at break     %

/

≥180

Mass change ratio       %

/

0~+25

10

Low-temperature performance   (-35℃/22h)

-30℃ No breaking

-30℃ No breaking

11

Compression permanent set PV3307  125℃X22h  %

≤85

≤85

12

Compression permanent set PV3307   23℃X94h  %

≤60

≤60

13

Copper corrosion V.W.2.8.1

Slight oxidation trace allowable

Slight oxidation trace allowable

14

Ozone aging (test piece not tested) 200pphm/46h/25℃/60/20%

No cracking 

No cracking 

15

Ozone aging  (after 125℃×94h) 200pphm/46h/25℃/60/20%  VW2.8.1

No cracking 

No cracking 

16

Ozone aging (after 125℃×94hmchine oil aging ) 200pphm/46h/25℃/60/20%      

No cracking 

No cracking 

17

Peel strength of external layer     N/mm

≥3.0

≥3.0


Return